QUINN AKRYLON XT PMMA
Subcategory: Acrylic; Thermoplastic
Material Notes: AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT sheets also combine the following excellent properties: brilliant transparency, very good weathering and ageing resistance, high surface stability/resistance, and good recyclability.Construction components - Light domes
- Partition walls
- Glazing
- Roofing
- Windows for caravans
Lighting - Prismatic control lenses
- Opal diffusers
Engineering components Advertising and Decorations - Letters
- Decorations
- Shop fittings
- Advertising panels
- Point of Purchase Displays
| Available Properties |
- Density
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Decomposition Temperature
- Refractive Index
- Haze
- Transmission, Visible
- Combustibility Grade
- Electrical Strength, kV/mm²
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|