QUINN XT PMMA

 

Subcategory: Acrylic; Thermoplastic

Material Notes:
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing resistance and remain color constant for years. High impact grades, QUINN XT610, XT620, XT630, have outstanding mechanical properties and excellent impact strength. Both QUINN XT sheets and all high impact grades can be used in contact with foodstuffs, as they meet all current European food control legislation. QUINN XT sheets and the high impact grades do not contain any toxic materials or heavy metals, which may cause environmental damage or health risks. It is insoluble in water, and not subject to hazardous materials identification. QUINN XT sheets and the high impact grades are easy to recycle.

Construction Components

  • Light domes
  • Partition walls
  • Door Glazing
  • Roofing
  • Skylights for caravans

Lighting

  • Lighting control lenses
  • Domestic light fittings

Engineering Components

  • Machine housings, machine safety covers

Advertising and Signage

  • Molded letters
  • Store displays
  • Shop fittings
  • Illuminated graphics panels

Other Applications

  • Containers
  • Lettering Templates
  • Solariums
  • Sound Barrier Walls

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Vicat Softening Point
  • Decomposition Temperature
  • Refractive Index
  • Transmission, Visible
  • Electrical Strength, kV/mm²
  • Forming Temperature, Air Pressure, °C
  • Forming Temperature, Vacuum, °C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。