Basell Lupolen® 5231 HX HDPE, Impact Grade
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: High Density Polyethylene
Material Notes: Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Tensile Impact Strength
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|