Basell Lupolen® V 2520 J Ethylene Vinyl Acetate, Film Grade
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Key Words: EVA
Material Notes: FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.