Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene

 

Subcategory: Polystyrene; Thermoplastic

Close Analogs:
Ineos Styrenics purchased this product line from BASF in 2005.

Material Notes:
Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applicable to polystyrene-based plastics, it is primarily used for extrusion/thermoforming. Avantra® 585K Q402 has the flow and surface gloss that make it suitable for coextrusion onto HIPS sheet used in durable goods applications like refrigerator liners and point of purchase displays. Unlike GPPS, Avantra® 585K Q402 produces a gloss cap that has excellent toughness with little sacrifice in surface appearance.

Information provided by Ineos Styrenics.

Available Properties
  • Density
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Rockwell L
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Gardner Impact
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Gloss
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。