BASF Luranyl® KR 2402 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
Subcategory: Styrene-Butadiene; Polyphenylene Ether/PPO; Thermoplastic
Key Words: PPE + SBS
Material Notes: Base grade with a balanced combination of impact strength and stiffness for parts calling for good heat deformation resistance (e.g. warm-air vents, coil formers, sheet and wheel covers).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|