BASF Procom® GC20H 250 Polypropylene
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Uses: car and truck fans and shrouds, car rear light housings, car radiator expansion tanks, car grills, domestic appliance components (e.g. washing machine tanks, impellers housings, etc.), textile bobbins and chemical plant, furniture frames.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|