BASF Ultradur® B 4040 G4 PBT + PET Blend, 20% Glass Fiber Reinforced
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Injection molding grade with 20% glass fibers for technical parts with excellent surface finish (e.g. oven- and car-door handles).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|