BASF Ultradur® S 4090 G2 PBT+ASA Blend, 10% Glass Fiber Reinforced
Subcategory: Polyester, TP; ASA Polymer; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Low-warpage, easy-flowing injection molding grade with 10% glass fibers for technical parts, for which dimensional stability is very important (e.g. housings, plug-and-socket connectors). Formerly called Ultrablend S KR 4090 G2.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|