BASF Ultraform® N2520 L Acetal
Subcategory: Acetal; Thermoplastic
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: This grade has low electrical surface resistivityData was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|