BASF Ultramid® A3WC4 Nylon 66, 20% Carbon Fiber Reinforced (Dry As Molded)
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Electrically conductive grade reinforced with 20% carbon fibers. Used for machinery elements and housings with high stiffness and dimensional stability, low density and favorable frictional behavior (e.g. connecting rods).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|