BASF Ultramid® A3WC4 Nylon 66, 20% Carbon Fiber Reinforced (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Electrically conductive grade reinforced with 20% carbon fibers. Used for machinery elements and housings with high stiffness and dimensional stability, low density and favorable frictional behavior (e.g. connecting rods).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|