BASF Ultramid® B35MF01 Nylon 6 (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Low viscosity, monomer-containing grade for making flexible monofilaments for fishing nets (thickness: 0.2 - 0.8 mm).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Elongation at Break
- Elongation at Yield
- Electrical Resistivity
- Surface Resistance
|
|
|
|
| Property Data |