BASF Ultramid® B3EG3 Nylon 6, 15% Glass Fiber Reinforced (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Glass fiber reinforced injection molding grade for housings with enhanced impact resistance (e.g. automotive mirror housings). Also used for the wheels of mountain bikes.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Dissipation Factor, Low Frequency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|