BASF Ultramid® B3M4 Nylon 6, Mineral Reinforced (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Mineral reinforced, easy flowing injection molding grade for high impact parts with good dimensional stability and low warpage tendency (e.g. wheel covers).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
|
|
|
|