BASF Ultramid® B3S Nylon 6 (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Easy flowing, finely crystalline injection molding grade for very fast processing. Uses include thin-walled technical parts (e.g. housing, fittings, grips, small parts, anchors and fixing clamps).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|