BASF Ultramid® B5 Nylon 6 (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: High-viscosity general-purpose grade for extruding high impact semi-finished products, tubes, profiles, blown film, sheet, strapping, thick monofilaments. Also used for blow molding (e.g. hydraulic oil reservoirs).Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|