BASF Ultramid® C3M8 Nylon 66/6, 40% Mineral Reinforced (Dry As Molded)
Subcategory: Nylon; Thermoplastic; Nylon 6/66; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Mineral-reinforced and stabilized injection molding grade for machinery components such as crown gears and small parts with high impact strength and low warpage.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|