BASF Ultramid® C3M8 Nylon 66/6, 40% Mineral Reinforced (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 6/66; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Mineral-reinforced and stabilized injection molding grade for machinery components such as crown gears and small parts with high impact strength and low warpage.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
|
|
|
|