BASF Ultramid® T KR 4355 G5 Nylon 6/6T (part. arom.), 25% Glass Fiber Reinforced (Dry As Molded)
Subcategory: Nylon; Thermoplastic; Nylon 66; Nylon, Aromatic; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Glass fiber reinforced injection-molding grade. High toughness, stiffness and strength, low water absorption, high melting point (295 °C). After the material has been conditioned, its mechanical properties remain stable up to 60 °C.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|