BASF Ultramid® T KR 4365 G5 Nylon 6/6T (part. arom.), 25% Glass Fiber Reinforced (At 50% RH)
Subcategory: Nylon; Thermoplastic; Nylon 66; Nylon, Aromatic; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Glass fiber reinforced, flame-retardant grade for injection molding. Good mechanical properties, high tracking resistance, only low tendency for deposits to form on electrical contacts, very resistant to electrolytic corrosion, resistant to solder baths.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Glass Temperature
|
|
|
|