BASF Ultrason® KR 4113 Polyethersulfone, 30% Filler ( Carbon Fiber, Graphite and PTFE Powder) (Dry As Molded)
Subcategory: Polyethersulfone; Thermoplastic; Polymer
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Compound based on PES with 30% filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improved Ultrason's tribological properties. In addition, this product has a very small expansion coefficient.Data was collected by ISO methods and provided by BASF.