BASF Vinidur® SZ 6465 PVC-Impact Grade
Subcategory: Vinyl; Thermoplastic
Close Analogs: BASF no longer produces PVC products. Their PVC product line is now a part of SolVin, a joint venture with Solvay.
Material Notes: PVC raw material, K-value 64, VC/AK impact-modified (11%), only processable when stabilized (compounded). Unplasticized. Used for manufacturing high-impact, weathering-resistant profile (esp. window profile). Parts made with this product are opaque.Data was collected by ISO methods and provided by BASF.
| Available Properties |
- Density
- Flammability, UL94
|
|
|
|