BASF Vinoflex® S 7114 PVC, Not Compounded
Subcategory: Vinyl; Thermoplastic
Close Analogs: BASF no longer produces Vinoflex® Their PVC product line is now a part of SolVin, a joint venture with Solvay.
Material Notes: PVC raw material, K-value 71, only processable after stabilization (compounding). Processing preferred with the addition of plasticizer for cable insulation, hose, profile, calendered film, floor covering, sheet and injection molded parts.Data was collected by ISO methods and provided by BASF.