BASF Vinuran® 3826 Modifier for PVC, Based on AK
Subcategory: Vinyl
Close Analogs: BASF no longer produces PVC products. Their PVC product line is now a part of SolVin, a joint venture with Solvay.
Material Notes: Modifier based on AK. For increasing the impact strength of PVC up to high-impact quality. Used for weather-resistant profile, sheet, film and injection molded parts. Parts containing this product are opaque. Add this product to PVC in recommended amounts of 5-15%. Data was collected by ISO methods and provided by BASF.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|