BASF Elastollan® 685A15N Polyester Type Polyurethane Elastomer

 

Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for extruded profile, sheet and film applications. They exhibit excellent abrasion resistance, toughness and transparency. With respect to processing they are generally easy to process and have a very wide processing window. In some cases it is as high as 25 to 30°C.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on molded plaques cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Available Properties
  • Density
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Tear Strength
  • Taber Abrasion, mg/1000 Cycles
  • Drying Temperature
  • Dry Time
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。