BASF Elastollan® S80A Polyester Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Tensile Set
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|