Ineos Styrenics Avantra 8550 Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Ineos Styrenics purchased this product line from BASF in 2005.
Material Notes: Ignition resistant grade of high impact polystyrene. It is free of polybrominated diphenylethers and meets UL94V-0 (@ 0.062"/1.6 mm min.) / 5VA (@ 0.125"/3.2 mm) ratings. It gives exceptional moldability while maintaining good mechanical and heat resistance properties. Information provided by BASF.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Gardner Impact
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|