Ineos Styrenics Polystyrene 148G (NAFTA)
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Ineos Styrenics purchased this product line from BASF in 2005.
Material Notes: High heat, easy flow general purpose polystyrene with excellent clarity. Designed for applications requiring a combination of fast processing with good strength and heat resistance. Information provided by BASF.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
|
|
|
|