Ineos Styrenics Polystyrene 168M (NAFTA)
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Ineos Styrenics purchased this product line from BASF in 2005.
Material Notes: High heat, high molecular weight general purpose polystyrene with low crystal clarity. It offers high stiffness for extrusion/thermoforming applications, especially for the food packaging. Information provided by BASF.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|