BASF Ultradur® B 4520 Q12 Uncolored PBT
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: An easy flowing PBT polyester resin that is well suited for thin wall injection molding applications. Information provided by BASF.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|