Ineos Styrenics 158K High-Heat Polystyrene Crystal Resin (Global)
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Ineos Styrenics purchased this product line from BASF in 2005.
Material Notes: Description: High-heat, high-molecular weight grades for a variety of applications, including medical devices and labware, cosmetics packaging, CD & DVD jewel boxes, food serviceware, and low-taste, low-odor products such as cook and cake trays as well as other oriented polystyrene (OPS) applications. Information provided by BASF.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|