Ineos Styrenics 495F High-Impact Polystyrene Resin (Global)
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Ineos Styrenics purchased this product line from BASF in 2005.
Material Notes: Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, packaging and food service, recreation equipment and sporting goods, medical devices and labware, office products, cosmetic and personal care products, and housewares. Information provided by BASF.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Gardner Impact @ 23°C
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Gloss
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|