Ineos Styrenics Avantra® 525K High Impact Styrenic Polymer (NAFTA)
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Ineos Styrenics purchased this product line from BASF in 2005.
Material Notes: Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office products, cosmetics and personal care products, building and construction, housewares, and furniture and furnishings. Information provided by BASF.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Gardner Impact @ 23°C
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Gloss
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|