Ineos Styrenics Avantra® 594E High Impact Styrenic Polymer (NAFTA)
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Ineos Styrenics purchased this product line from BASF in 2005.
Material Notes: Description: Avantra® 594E is a super high-impact polystyrene grade that delivers excellent processing efficiency along with toughness and high gloss in a wide variety of injection molding applications such as consumer electronics, office equipment, building & construction, housewares, office products, cosmetics & personal care products, recreation equipment & sporting goods, toys, and furniture & furnishings. Information provided by BASF.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Gardner Impact @ 23°C
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Gloss
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|