SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Seals, compressors, pumps, bearings Information provided by SGL Carbon Group
| Available Properties |
- Density
- Open Porosity
- Hardness, Rockwell R
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
- Maximum Service Temperature, Inert
|
|
|
|