Shakespeare Resistat® F9416 Merge M040 Nylon 66 Monofilament
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Resistat F9416, MERGE M040 is composed of forty filaments of conductive nylon 6,6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section with a coating thickness of approximately 1 micron. The yarn color is black. Resistat is used for carpeting, ESD garments, and industrial belting and brushes. Information provided by Shakespeare Company.
| Available Properties |
- Fiber Count
- Tenacity
- Elongation at Break
- Electrical Resistivity
- Melting Point
|
|
|
|