Shakespeare Resistat® F9116 Merge A012 Nylon 66 Monofilament
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Resistat F9116, MERGE A012 is a 16 denier per filament nylon 6,6 chopped fiber. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section with a coating thickness of approximately 1 micron. Resistat is used for carpeting, ESD garments, and industrial belting and brushes. Information provided by Shakespeare Company.
| Available Properties |
- Fiber Count
- Tenacity
- Elongation at Break
- Electrical Resistivity
- Melting Point
|
|
|
|
| Property Data |