Shakespeare Resistat® F9216 Merge F040 Nylon 66 Monofilament
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Resistat F2416, MERGE F040 is a nylon 6,6 multifilament yarn. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section with a coating thickness of approximately 1 micron. It is available with a 40 filaments version yielding a total of 670 denier. The yarn color is black. Resistat is used for carpeting, ESD garments, and industrial belting and brushes. Information provided by Shakespeare Company.
| Available Properties |
- Fiber Count
- Tenacity
- Elongation at Break
- Electrical Resistivity
- Melting Point
|
|
|
|