Shakespeare WonderThread® SN-38 High tenacity TEX# 45 Nylon Industrial Sewing Thread
Subcategory: Nylon; Thermoplastic
Material Notes: Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping Bags Information provided by Shakespeare Company.
| Available Properties |
- Fiber Count
- Tensile Strength @ Break
- Tenacity
- Elongation at Yield
- Shrinkage
|
|
|
|