Shakespeare WP-315 diameter 0.2 mm Weft Polyester Monofilament
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Paper Machine Clothing Monofilament
- Standard molecular weight
- Polyester
- For endless machine direction use
- High shrinkage
Information provided by Shakespeare Company.
| Available Properties |
- Elongation at Break
- Elongation at Yield
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|