Shakespeare WN-102 diameter 0.5 mm Nylon 66 Monofilament
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Paper Machine Clothing Monofilament
- Nylon 6,6
- Moderate Modulus
- Low shrinkage
Information provided by Shakespeare Company.
| Available Properties |
- Elongation at Yield
- Shrinkage
|
|
|
|