Shakespeare HPA-14 diameter 0.7 mm PPS Monofilament
Subcategory: Polyphenylene Sulfide; Thermoplastic
Material Notes: Paper Machine Clothing Monofilament
- Chemical resistant
- High service temperature
- Non-hydrolyzing
- Warp yarn
- High shrinkage
Information provided by Shakespeare Company.
| Available Properties |
- Tensile Strength @ Break
- Elongation at Break
- Elongation at Yield
- Shrinkage
|
|
|
|