Shakespeare Isocor™ TT52SI Nylon 6 Terpolymer
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Isocor™ TT52SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocor™ TT52SI is easily processed and has a wide range of applications due to its physical properties, chemical resistance, and lower melt temperatures. Used for polymer additives, pigment carriers, and specialty adhesives. Information provided by Shakespeare Company.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Volume Resistivity
- Melting Point
|
|
|
|