Shakespeare Isocor™ HG26SI medium viscosity PA-612
Subcategory: Nylon; Thermoplastic; Nylon 612
Material Notes: Isocor™ HG26SI is a medium viscosity PA-612 based nylon. This resin is specifically suited for applications requiring low moisture regain and greater dimensional stability. Isocor™ HG26SI is also used in applications requiring good electrical insulation properties. This resin can be processed using conventional techniques. Used for cable jacketing, bristles, extrusion, films, and tubing. Information provided by Shakespeare Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Tensile Modulus
- Gardner Impact @ 23°C
- Izod Impact, Notched
- Melting Point
- Moisture Content
|
|
|
|