Shakespeare Isocor™ HW115SI Nylon 610
Subcategory: Nylon; Thermoplastic; Nylon 610
Material Notes: Isocor™ HW115SI is a high viscosity PA-610. This resin is specifically suited for applications requiring low moisture absorption and greater dimensional stability, and improved abrasion resistance. This resin can be processed using conventional techniques. Used for cable jacketing, monofilaments / bristles, film extrusions, and automotive tubing. Information provided by Shakespeare Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Taber Abrasion, mg/1000 Cycles
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|