Shakespeare Isocor™ HW29TL Nylon 610
Subcategory: Nylon; Thermoplastic; Nylon 610
Material Notes: Isocor™ HW29TL is an ultra low viscosity PA-610 with excellent melt flow characteristics. Isocor™ HW29TL is specifically formulated for thin wall or high speed injection molding applications. This resin is suitable for applications requiring low moisture absorption and greater dimensional stability. This resin can be processed using conventional techniques. Used for thin-wall injection molding, electrical connectors, small parts-high output Information provided by Shakespeare Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Taber Abrasion, mg/1000 Cycles
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|