Shakespeare Isocor™ SVP4007 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Isocor™ SVP4007 is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed using conventional techniques. Used for profile extrusions, film extrusions, flexible tubing, fiber and filaments. Information provided by Shakespeare Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength @ Break
- Tensile Modulus
- Gardner Impact @ 23°C
- Izod Impact, Notched
- Melting Point
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|