Shuman SP920 Black Polycarbonate SP 900 Series
Subcategory: Polycarbonate; Thermoplastic
Close Analogs: Data provided by the manufacturer.
Material Notes: Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.