Sibur 21030-PM1 Polypropylene with Low Muddiness
Subcategory: Polypropylene; Thermoplastic
Material Notes: For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products.
| Available Properties |
- Melt Index of Compound
- Collected Volatile Condensable Material
- Tensile Strength, Yield
- Modulus of Elasticity
- Izod Impact, Notched (ISO)
- Muddiness of Film
- Spread Flow Batch Error
|
|
|
|